MatWeb, The Online Materials Database

Degussa AG Vestamid® L-R2-GF25 25% Glass, Antistatic, Black, Electrically Conductive Nylon 12


Subcategory: Filled/Reinforced Thermoplastic; Nylon; Nylon 12; Polymer; Thermoplastic

Key Words: PA12, MHZ,18-060,GF25

Material Notes:
Description: Medium-viscosity,25% chopped strands, heat- and light-stabilized

Applications: Antistatic and electrically conductive moldings or extrudates for use in areas prone to explosions such as coal mining and other industries; e.g., housings for explosion-protected measuring equipment or for electric switches, ventilation fans for electric motors, chair castors, loudspeaker boxes, telephone and radio equipment, profiles for guide rails in assembly lines in the electronics industry. Also with electric shock protection.

Information provided by degussa.

Physical PropertiesMetricEnglishComments
Density1.27 g/cc0.0459 lb/in³ ISO 1183
Moisture Absorption at Equilibrium0.5 %0.5 % 23°C/50% R.H. (1mm); ISO 62
Water Absorption at Saturation1.2 %1.2 % 1 mm; ISO 62
Linear Mold Shrinkage0.002 cm/cm0.002 in/in 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
Linear Mold Shrinkage, Transverse0.011 cm/cm0.011 in/in 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)

Mechanical Properties
Tensile Strength at Break120 MPa17400 psi ISO 527-1/2
Elongation at Break5 %5 % ISO 527-1/2
Tensile Modulus6.5 GPa943 ksi ISO 527-1/2
Charpy Impact Unnotched7.5 J/cm²35.7 ft-lb/in² 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp1.1 J/cm²5.24 ft-lb/in² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low Temp7 J/cm²33.3 ft-lb/in² -30°C; ISO 179/1eU
Charpy Impact, Notched1.2 J/cm²5.71 ft-lb/in² 23°C; ISO 179/1eA

Electrical Properties
Volume Resistivity100 ohm-cm100 ohm-cm IEC 60093
Insulation Resistance100 ohm100 ohm Isolation Resistance (ROE DIN 43582:1983/VDE 0303 part 3; IEC 60167

Thermal Properties
CTE, linear 20°C100 µm/m-°C55.6 µin/in-°F 23-55°C (45x15x10 mm); ISO 11359
Melting Point178 °C352 °F Peak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi)175 °C347 °F ISO 75
Deflection Temperature at 1.8 MPa (264 psi)170 °C338 °F ISO 75
Vicat Softening Point170 °C338 °F 50N; ISO 306
Vicat Softening Point175 °C347 °F 10N; ISO 306
Flammability, UL94HBHB 3.2 mm
Flammability, UL94HBHB 1.6 mm

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.