Degussa AG Vestamid® LX9007 Nylon 12


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Key Words: PA12, EL,22-010

Material Notes:
Description: High-viscosity, light-stabilized

Applications: Transparent, scratch-resistant, and printable decorative films

Information provided by degussa.

Physical PropertiesMetricEnglishComments
Density1.01 g/cc0.0365 lb/in³ ISO 1183
Moisture Absorption at Equilibrium0.7 %0.7 % 23°C/50% R.H. (1mm); ISO 62
Water Absorption at Saturation1.6 %1.6 % 1 mm; ISO 62
Linear Mold Shrinkage0.012 cm/cm0.012 in/in 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)
Linear Mold Shrinkage, Transverse0.014 cm/cm0.014 in/in 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2)

Mechanical Properties
Tensile Strength, Yield47 MPa6820 psi ISO 527-1/2
Elongation at BreakMin 50 %Min 50 % ISO 527-1/2
Elongation at Yield5 %5 % ISO 527-1/2
Tensile Modulus1.4 GPa203 ksi ISO 527-1/2
Charpy Impact UnnotchedNBNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.9 J/cm²4.28 ft-lb/in² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempNBNB -30°C; ISO 179/1eU
Charpy Impact, Notched1.6 J/cm²7.61 ft-lb/in² 23°C; ISO 179/1eA

Electrical Properties
Volume Resistivity1e+015 ohm-cm1e+015 ohm-cm IEC 60093
Dielectric Constant33 23°C/1 MHz; IEC 60250
Dielectric Constant, Low Frequency3.73.7 23°C/100 Hz; IEC 60250
Dielectric Strength26 kV/mm660 kV/in K20/P50; IEC 60243-1
Dissipation Factor0.0260.026 23°C/1 MHz; IEC 60250
Dissipation Factor, Low Frequency0.0450.045 23°C/100 Hz; IEC 60250
Comparative Tracking IndexMin 600 VMin 600 V Test Solution A, 50 drops; IEC 60112
Comparative Tracking Index600 V600 V Test Solution A, 100 drops; IEC 60112

Thermal Properties
CTE, linear 20°C140 µm/m-°C77.8 µin/in-°F 23-55°C (45x15x10 mm); ISO 11359
Melting Point178 °C352 °F Peak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi)110 °C230 °F ISO 75
Deflection Temperature at 1.8 MPa (264 psi)50 °C122 °F ISO 75
Vicat Softening Point140 °C284 °F 50N; ISO 306
Vicat Softening Point170 °C338 °F 10N; ISO 306
Flammability, UL94HBHB 3.2 mm
Flammability, UL94HBHB 1.6 mm

Descriptive Properties
Electrolytic CorrosionA1 Step IEC 60426

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.