Degussa AG Vestamid® X4863 Nylon 12


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Key Words: PA12-HI,MHL,18-010

Material Notes:
Description: Medium-viscosity, increased low-temperature impact strength, heat- and light-stabilized

Applications: Components for ski bindings

Information provided by degussa.

Physical PropertiesOriginal ValueComments
Density1.01 g/cc ISO 1183
Moisture Absorption at Equilibrium0.5 % 23°C/50% R.H. (1mm); ISO 62
Water Absorption at Saturation1.4 % 1 mm; ISO 62

Mechanical Properties
Tensile Strength, Yield36 MPa ISO 527-1/2
Elongation at BreakMin 50 % ISO 527-1/2
Elongation at Yield7 % ISO 527-1/2
Tensile Modulus1.1 GPa ISO 527-1/2
Charpy Impact UnnotchedNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp2.2 J/cm² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempNB -30°C; ISO 179/1eU
Charpy Impact, Notched6.5 J/cm² 23°C; ISO 179/1eA

Electrical Properties
Volume Resistivity1e+016 ohm-cm IEC 60093
Dielectric Constant3.1 23°C/1 MHz; IEC 60250
Dielectric Constant, Low Frequency3.3 23°C/100 Hz; IEC 60250
Dielectric Strength30 kV/mm K20/P50; IEC 60243-1
Dissipation Factor0.022 23°C/1 MHz; IEC 60250
Dissipation Factor, Low Frequency0.035 23°C/100 Hz; IEC 60250
Comparative Tracking IndexMin 600 V Test Solution A, 50 drops; IEC 60112
Comparative Tracking Index600 V Test Solution A, 100 drops; IEC 60112

Thermal Properties
CTE, linear 20°C140 µm/m-°C 23-55°C (45x15x10 mm); ISO 11359
Melting Point178 °C Peak Temperature; ISO 3146, ISO 11357
Deflection Temperature at 0.46 MPa (66 psi)110 °C ISO 75
Deflection Temperature at 1.8 MPa (264 psi)50 °C ISO 75
Vicat Softening Point120 °C 50N; ISO 306
Vicat Softening Point170 °C 10N; ISO 306
Flammability, UL94HB 3.2 mm
Flammability, UL94HB 1.6 mm

Descriptive Properties
Electrolytic CorrosionA1 Step IEC 60426

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.