Degussa AG Vestamid® X7163 High Viscosity, Heat Stabilized, Graphite Filled Nylon 12


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Material Notes:
Description: VESTAMID X7163 black is a graphite-filled and heat-stabilized compound for extrusion. Its improved properties of sliding friction make it most suitable for the production of push-pull cable liners. Further advantages of VESTAMID X7163black are the characteristic properties of PA 12like small water absorption, good dimensional stability and nearly constant mechanical properties at changing ambient humidity.

Information provided by degussa.

Physical PropertiesOriginal ValueComments
Density1.08 g/cc ISO 1183

Mechanical Properties
Hardness, Shore D75 ISO 868
Tensile Strength, Yield47 MPa ISO 527-1/2
Elongation at Break37 % ISO 527-1/2
Elongation at Yield5.4 % ISO 527-1/2
Tensile Modulus2.35 GPa ISO 527-1/-2
Charpy Impact Unnotched9.5 J/cm² 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.4 J/cm² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low Temp9 J/cm² -30°C; ISO 179/1eU
Charpy Impact, Notched0.57 J/cm² 23°C; ISO 179/1eA

Electrical Properties
Volume Resistivity1e+014 ohm-cm IEC 60093
Surface Resistance1e+013 ohm IEC 60093
Dielectric Constant5 1 MHz; IEC 60250
Dielectric Constant, Low Frequency6 100 Hz; IEC 60250
Dielectric Strength22 kV/mm K20/P50; IEC 60243-1
Dissipation Factor45 1 MHz; IEC 60250
Dissipation Factor, Low Frequency65 100 Hz; IEC 60250
Comparative Tracking Index275 V 100 drops value; IEC 60112
Comparative Tracking Index300 V Test Solution A CTI; IEC 60112

Thermal Properties
CTE, linear 20°C91 µm/m-°C Longitudinal, 23-55°C; ISO 11359, DIN 53752
CTE, linear 20°C Transverse to Flow87 µm/m-°C 23-55°C; ISO 11359, DIN 53752
Deflection Temperature at 0.46 MPa (66 psi)140 °C ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi)50 °C ISO 75-1/-2
Vicat Softening Point160 °C Method B, 50 N; ISO 306
Vicat Softening Point175 °C Method A, 10 N; ISO 306
Flammability, UL94HB 1.6 mm; IEC 60695
Flammability, UL94HB 3.2 mm; IEC 60695

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.