Degussa AG Vestamid® X7166 Flame Retardant Nylon 12
Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic
Key Words: PA12,KFH,12-020
Material Notes: Description: Low-viscosity resin with flame retardant, free of halogen and phosphorus, UL 94-V0/V2, with processing aid Applications: Wire insulation Information provided by degussa.
Physical Properties | Metric | English | Comments |
|
Density | 1.06 g/cc | 0.0383 lb/in³ | ISO 1183 |
Moisture Absorption at Equilibrium | 0.6 % | 0.6 % | 23°C/50% R.H. (1mm); ISO 62 |
Water Absorption at Saturation | 1.3 % | 1.3 % | 1 mm; ISO 62 |
Linear Mold Shrinkage | 0.011 cm/cm | 0.011 in/in | 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2) |
Linear Mold Shrinkage, Transverse | 0.011 cm/cm | 0.011 in/in | 127x12.7x3.2 mm (processing cond. acc. To ISO 1874-2) |
Mechanical Properties |
|
Tensile Strength, Yield | 47 MPa | 6820 psi | ISO 527-1/2 |
Elongation at Break | Min 50 % | Min 50 % | ISO 527-1/2 |
Elongation at Yield | 5 % | 5 % | ISO 527-1/2 |
Tensile Modulus | 1.8 GPa | 261 ksi | ISO 527-1/2 |
Charpy Impact Unnotched | 6.5 J/cm² | 30.9 ft-lb/in² | 23°C; ISO 179/1eU |
Charpy Impact, Notched, Low Temp | 0.5 J/cm² | 2.38 ft-lb/in² | -30°C; ISO 179/1eA |
Charpy Impact, Unnotched Low Temp | 8 J/cm² | 38.1 ft-lb/in² | -30°C; ISO 179/1eU |
Charpy Impact, Notched | 0.3 J/cm² | 1.43 ft-lb/in² | 23°C; ISO 179/1eA |
Electrical Properties |
|
Volume Resistivity | 1e+014 ohm-cm | 1e+014 ohm-cm | IEC 60093 |
Dielectric Constant | 3.6 | 3.6 | 23°C/1 MHz; IEC 60250 |
Dielectric Strength | 28 kV/mm | 711 kV/in | K20/P50; IEC 60243-1 |
Dissipation Factor | 0.034 | 0.034 | 23°C/1 MHz; IEC 60250 |
Comparative Tracking Index | Min 600 V | Min 600 V | Test Solution A, 50 drops; IEC 60112 |
Comparative Tracking Index | 600 V | 600 V | Test Solution A, 100 drops; IEC 60112 |
Thermal Properties |
|
Melting Point | 178 °C | 352 °F | Peak Temperature; ISO 3146, ISO 11357 |
Deflection Temperature at 0.46 MPa (66 psi) | 140 °C | 284 °F | ISO 75 |
Deflection Temperature at 1.8 MPa (264 psi) | 50 °C | 122 °F | ISO 75 |
Vicat Softening Point | 150 °C | 302 °F | 50N; ISO 306 |
Vicat Softening Point | 175 °C | 347 °F | 10N; ISO 306 |
Flammability, UL94 | V-0 | V-0 | 3.2 mm |
Flammability, UL94 | V-0 | V-0 | 1.6 mm |
Descriptive Properties | |
Electrolytic Corrosion | A1 Step | IEC 60426 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |