Degussa AG Vestamid®®/Trogamid® RD 5080 HNBR Rubber/Plastic Composite


Subcategory: Polymer; Thermoplastic

Material Notes:
Formulation
Zetpol® 3110100
Carbon Black N 55065
Rhenosin® W-75910
ZnO2
HVA 24
Perkadox® 14/407

Information provided by degussa.

Physical PropertiesOriginal ValueComments
Viscosity Measurement0.32 min, Reometer at 170°C t10
Viscosity Measurement2 min, Reometer at 170°C t90

Mechanical Properties
Hardness, Shore A79 23°C
Tensile Strength at Break21.2 MPa 
Elongation at Break154 % 
100% Modulus0.0128 GPa 
Rebound32 % 23°C

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.