Degussa AG Vestamid® LX9104 Nylon 12


Subcategory: Nylon; Nylon 12; Polymer; Thermoplastic

Material Notes:
Description: VESTAMID LX9104 is a halogen-free flame-retardant and flexible PA 12 compound of flammability class V-0 at0.8mm according to UL 94 and a LOI of 28%.

Information provided by degussa.

Physical PropertiesMetricEnglishComments
Density1.12 g/cc0.0405 lb/in³ ISO 1183

Mechanical Properties
Tensile Strength, Yield27 MPa3920 psi ISO 527-2/1A
Elongation at BreakMin 50 %Min 50 % ISO 527-2/1A
Elongation at Yield24 %24 % ISO 527-2/1A
Tensile Modulus0.75 GPa109 ksi ISO 527-1/2
Charpy Impact UnnotchedNBNB 23°C; ISO 179/1eU
Charpy Impact, Notched, Low Temp0.3 J/cm²1.43 ft-lb/in² -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low Temp15 J/cm²71.4 ft-lb/in² -30°C, Partial Break; ISO 179/1eU
Charpy Impact, Notched0.6 J/cm²2.86 ft-lb/in² 23°C; ISO 179/1eA

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.