MatWeb, The Online Materials Database

LNP (SABIC Innovative Plastics) VALOX® VC112 Polybutylene Terephthalate


Subcategory: Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:

  • Forms: Pellets

Information provided by LNP, a GE Plastics Company.

Physical PropertiesMetricEnglishComments
Specific Gravity1.44 g/cc0.052 lb/in³ ASTM D792
Linear Mold Shrinkage0.002 - 0.003 cm/cm0.002 - 0.003 in/in 3.20 mm; ASTM D955
Linear Mold Shrinkage0.007 - 0.008 cm/cm0.007 - 0.008 in/in 6.40 mm; ASTM D955

Mechanical Properties
Tensile Strength, Yield118 MPa17100 psi ASTM D638
Flexural Modulus7.35 GPa1070 ksi ASTM D790
Flexural Strength177 MPa25700 psi ASTM D790
Izod Impact, Notched0.49 J/cm0.918 ft-lb/in ASTM D256

Electrical Properties
Surface Resistance100000 - 1e+008 ohm100000 - 1e+008 ohm ASTM D257

Thermal Properties
CTE, linear 20°C65 µm/m-°C36.1 µin/in-°F TMA, -30°C to 30°C
Deflection Temperature at 0.46 MPa (66 psi)180 °C356 °F Unannealed (3.20 mm); ASTM D648

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.