MatWeb, The Online Materials Database
LNP (SABIC Innovative Plastics) ULTEM® SMU5831 Polyetherimide, 30% Carbon\Glass\Mineral Reinforced
Subcategory: Filled/Reinforced Thermoplastic; Polyetherimide; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: ESD characteristics for ultra high-heat applications. Will be UC3010H. - Features: High Heat Resistance
- Forms: Pellets
- Processing Method: Injection Molding
Information provided by LNP, a GE Plastics Company.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.48 g/cc | 0.0535 lb/in³ | ASTM D792 |
Mechanical Properties |
|
Tensile Strength at Break | 131 MPa | 19000 psi | Type I, 5 mm/min; ASTM D638 |
Elongation at Break | 3.9 % | 3.9 % | Type I, 5 mm/min; ASTM D638 |
Flexural Modulus | 10.3 GPa | 1490 ksi | (102 mm Span) 3mm/min; ASTM D790 |
Flexural Yield Strength | 157 MPa | 22800 psi | (102 mm Span) 3mm/min; ASTM D790 |
Izod Impact, Notched | 0.374 J/cm | 0.701 ft-lb/in | ASTM D256 |
Electrical Properties |
|
Surface Resistance | 100000 ohm | 100000 ohm | ASTM D257 |
Static Decay | Max 0.01 sec | Max 0.01 sec | 5000V to <50V; FTMS101B |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 223 °C | 433 °F | Unannealed (6.35 mm); ASTM D648 |
Processing Properties |
|
Rear Barrel Temperature | 360 - 421 °C | 680 - 790 °F | |
Middle Barrel Temperature | 371 - 421 °C | 700 - 790 °F | |
Front Barrel Temperature | 382 - 427 °C | 720 - 801 °F | |
Nozzle Temperature | 377 - 421 °C | 711 - 790 °F | |
Melt Temperature | 382 - 427 °C | 720 - 801 °F | |
Mold Temperature | 135 - 163 °C | 275 - 325 °F | |
Drying Temperature | 149 °C | 300 °F | |
Dry Time | Max 24 hour | Max 24 hour | |
Moisture Content | 0.02 % | 0.02 % | Suggested |
Back Pressure | 0.345 - 0.689 MPa | 50 - 99.9 psi | |
Clamp Pressure | 41 - 69 MPa | 5950 - 10000 psi | |
Shot Size | 40 - 60 % | 40 - 60 % | Suggested |
Vent Depth | 0.0025 - 0.0076 cm | 0.000984 - 0.00299 in | |
Screw Speed | 40 - 70 rpm | 40 - 70 rpm | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|