Physical PropertiesOriginal ValueComments
Specific Gravity1.39 g/cc ASTM D792
Filler Content5 % Primary Additive
Linear Mold Shrinkage0.006 - 0.008 cm/cm 1/8 in (3.2 mm); ASTM D955

Mechanical Properties
Tensile Strength @ Break13000 psi ASTM D638
Elongation at Break6 - 8 % ASTM D638
Tensile Modulus500000 psi ASTM D638
Flexural Modulus500000 psi ASTM D638
Flexural Yield Strength19000 psi ASTM D790
Izod Impact, Unnotched21 ft-lb/in 1/8 in (3.2 mm); ASTM D4812
Izod Impact, Notched1 ft-lb/in 1/8 in (3.2 mm); ASTM D256

Thermal Properties
Flammability, UL94V-0 1/16 in (1.5 mm)

Processing Properties
Melt Temperature650 - 710 °F 
Mold Temperature275 - 350 °F 
Drying Temperature300 °F 6 hrs
Moisture Content0.04 % 
Dew Point-25 °F 
Injection Pressure10000 - 15000 psi 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.