MatWeb, The Online Materials Database

RTP Company RTP 1400 Polyethersulfone (PES)


Subcategory: Polyethersulfone; Polymer; Thermoplastic

Physical PropertiesMetricEnglishComments
Specific Gravity1.37 g/cc0.0495 lb/in³ ASTM D792
Water Absorption0.54 %0.54 % 24 hrs; 23°C; ASTM D570
Linear Mold Shrinkage0.007 cm/cm0.007 in/in 1/8 in (3.2 mm); ASTM D955
Melt Flow80 g/10 min80 g/10 min 385°C/2160 kg; ASTM D1238

Mechanical Properties
Tensile Strength @ Break82.7 MPa12000 psi ASTM D638
Elongation at Break30 %30 % ASTM D638
Tensile Modulus2.69 GPa390 ksi ASTM D638
Flexural Modulus2.9 GPa420 ksi ASTM D638
Flexural Yield Strength111 MPa16100 psi ASTM D790
Izod Impact, Notched0.694 J/cm1.3 ft-lb/in 1/8 in (3.2 mm); ASTM D256

Electrical Properties
Volume ResistivityMin 1e+012 ohm-cmMin 1e+012 ohm-cm ASTM D257
Dielectric Constant3.53.5 1 MHz; Dry; ASTM D150
Dielectric Strength15 kV/mm380 V/mil S/T; in oil; ASTM D149
Dissipation Factor0.00560.0056 1 MHz; Dry; ASTM D150

Thermal Properties
CTE, linear 68°F48.6 µm/m-°C27 µin/in-°F Flow Direction; ASTM E831
Deflection Temperature at 1.8 MPa (264 psi)203 °C398 °F ASTM D648
Flammability, UL94V-0V-0 1/16 in (1.5 mm)

Processing Properties
Melt Temperature343 - 377 °C650 - 710 °F 
Mold Temperature135 - 177 °C275 - 350 °F 
Drying Temperature149 °C300 °F 6 hrs
Moisture Content0.04 %0.04 % 
Dew Point-31.7 °C-25 °F 
Injection Pressure68.9 - 103 MPa10000 - 15000 psi 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.