RTP Company RTP 1485 N Polyethersulfone (PES) Carbon Fiber - High Viscosity
Subcategory: Polyethersulfone; Polymer; Thermoplastic
| Physical Properties | Metric | English | Comments |
|
| Specific Gravity | 1.45 g/cc | 0.0524 lb/in³ | ASTM D792 |
| Filler Content | 30 % | 30 % | Primary Additive |
| Water Absorption | 0.35 % | 0.35 % | 24 hrs; 23°C; ASTM D570 |
| Linear Mold Shrinkage | 0.001 cm/cm | 0.001 in/in | 1/8 in (3.2 mm); ASTM D955 |
Mechanical Properties |
|
| Tensile Strength @ Break | 210 MPa | 30500 psi | ASTM D638 |
| Elongation at Break | 1.5 % | 1.5 % | ASTM D638 |
| Tensile Modulus | 23.4 GPa | 3400 ksi | ASTM D638 |
| Flexural Modulus | 20 GPa | 2900 ksi | ASTM D638 |
| Flexural Yield Strength | 303 MPa | 44000 psi | ASTM D790 |
| Izod Impact, Unnotched | 6.14 J/cm | 11.5 ft-lb/in | 1/8 in (3.2 mm); ASTM D4812 |
| Izod Impact, Notched | 0.854 J/cm | 1.6 ft-lb/in | 1/8 in (3.2 mm); ASTM D256 |
Electrical Properties |
|
| Volume Resistivity | Max 100000 ohm-cm | Max 100000 ohm-cm | ASTM D257 |
Thermal Properties |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 210 °C | 410 °F | ASTM D648 |
| Flammability, UL94 | V-0 | V-0 | 1/16 in (1.5 mm) |
Processing Properties |
|
| Melt Temperature | 343 - 377 °C | 650 - 710 °F | |
| Mold Temperature | 135 - 177 °C | 275 - 350 °F | |
| Drying Temperature | 149 °C | 300 °F | 6 hrs |
| Moisture Content | 0.04 % | 0.04 % | |
| Dew Point | -31.7 °C | -25 °F | |
| Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |