MatWeb, The Online Materials Database

RTP Company ESD A 1480 Polyethersulfone (PES) Carbon Fiber - ESD Protection - Static Dissipative


Subcategory: Polyethersulfone; Polymer; Thermoplastic

Physical PropertiesOriginal ValueComments
Specific Gravity1.38 g/cc ASTM D792
Linear Mold Shrinkage0.003 cm/cm 1/8 in (3.2 mm); ASTM D955

Mechanical Properties
Tensile Strength @ Break17000 psi ASTM D638
Elongation at Break2 - 3 % ASTM D638
Tensile Modulus1e+006 psi ASTM D638
Flexural Modulus1e+006 psi ASTM D638
Flexural Yield Strength25000 psi ASTM D790
Izod Impact, Unnotched9 ft-lb/in 1/8 in (3.2 mm); ASTM D4812
Izod Impact, Notched1 ft-lb/in 1/8 in (3.2 mm); ASTM D256

Electrical Properties
Volume Resistivity1000 - 9.9e+009 ohm-cm ASTM D257
Surface Resistance10000 - 9.9e+011 ohm ESD S11.11
Surface Resistivity per Square100000 - 9.9e+012 ohm ASTM D257; ESD S11.11
Static DecayMax 2 sec FTMS101C; 4046.1

Processing Properties
Melt Temperature650 - 710 °F 
Mold Temperature275 - 350 °F 
Drying Temperature300 °F 6 hrs
Moisture Content0.04 % 
Dew Point-25 °F 
Injection Pressure10000 - 15000 psi 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.