MatWeb, The Online Materials Database
RTP Company RTP 1403 B Polyethersulfone (PES) Glass Fiber 20%
Subcategory: Polyethersulfone; Polymer; Thermoplastic
Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Material Notes: Glass Fiber 20% Comments: Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company.
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.51 g/cc | ASTM D792 |
| Filler Content | 20 % | |
| Water Absorption | 0.4 % | 24 hours at 23°C; ASTM D570 |
| Linear Mold Shrinkage | 0.002 cm/cm | 1/8 inch (3.18 mm) section; ASTM D955 |
| Linear Mold Shrinkage, 6.35 mm section | 0.003 cm/cm | 1/4 inch (6.35 mm) section; ASTM D955 |
Mechanical Properties |
|
| Tensile Strength, Ultimate | 19000 psi | ASTM D638 |
| Elongation at Break | 2.9 % | ASTM D638 |
| Modulus of Elasticity | 1000 ksi | ASTM D638 |
| Flexural Modulus | 800 ksi | ASTM D790 |
| Flexural Yield Strength | 27000 psi | ASTM D790 |
| Compressive Yield Strength | 20000 psi | ASTM D695 |
| Izod Impact, Unnotched | 11 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
| Izod Impact, Notched | 1.4 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
Electrical Properties |
|
| Electrical Resistivity | 1e+016 ohm-cm | ASTM D257 |
| Dielectric Constant | 3.9 | 1 MHz, Dry; ASTM D150 |
| Dielectric Strength | 375 V/mil | S/T; ASTM D149 |
| Dissipation Factor | 0.007 | 1 MHz, Dry; ASTM D150 |
Thermal Properties |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 410 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 405 °F | ASTM D648 |
| Flammability, UL94 | V-0 | (V-0) at 1/16 in (1.59 mm); Per testing by RTP Company; ASTM D3801 |
Processing Properties |
|
| Processing Temperature | 650 - 690 °F | |
| Mold Temperature | 275 - 350 °F | |
| Injection Pressure | 10000 - 15000 psi | |
Descriptive Properties | |
| Color | Natural/Black | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from