MatWeb, The Online Materials Database

RTP Company RTP 1405 HF TFE 15 Polyethersulfone (PES) Glass Fiber 30% - PTFE 15% - High Flow


Subcategory: Polyethersulfone; Polymer; Thermoplastic

Close Analogs:
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Material Notes:
Glass Fiber 30% - PTFE 15% - High Flow

Comments:

  • Glass Fiber
  • PTFE Lubricated
  • High Flow

Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.

Information provided by RTP Company.

Physical PropertiesOriginal ValueComments
Specific Gravity1.69 g/cc ASTM D792
Filler Content30 % 
Linear Mold Shrinkage0.005 cm/cm 1/8 inch (3.18 mm) section; ASTM D955

Mechanical Properties
Tensile Strength, Ultimate16000 psi ASTM D638
Elongation at Break1.4 % ASTM D638
Modulus of Elasticity1500 ksi ASTM D638
Flexural Modulus1300 ksi ASTM D790
Flexural Yield Strength25000 psi ASTM D790
Izod Impact, Unnotched9 ft-lb/in 1/8 in (3.18 mm) section; ASTM D256
Izod Impact, Notched2 ft-lb/in 1/8 in (3.18 mm) section; ASTM D256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)400 °F ASTM D648

Processing Properties
Processing Temperature650 - 690 °F 
Mold Temperature275 - 350 °F 
Injection Pressure10000 - 15000 psi 

Descriptive Properties
ColorNatural/Black 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.