RTP Company RTP 1405 L Polyethersulfone (PES) Glass Fiber 30% - Lubricated


Subcategory: Polyethersulfone; Polymer; Thermoplastic

Close Analogs:
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Material Notes:
Glass Fiber 30% - Lubricated

Comments:

  • Glass Fiber
  • Lubricated

Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.

Information provided by RTP Company.

Physical PropertiesMetricEnglishComments
Specific Gravity1.59 g/cc0.0574 lb/in³ ASTM D792
Filler Content30 %30 % 
Water Absorption0.35 %0.35 % 24 hours at 23°C; ASTM D570
Linear Mold Shrinkage0.001 cm/cm0.001 in/in 1/8 inch (3.18 mm) section; ASTM D955
Linear Mold Shrinkage, 6.35 mm section0.002 cm/cm0.002 in/in 1/4 inch (6.35 mm) section; ASTM D955

Mechanical Properties
Hardness, Rockwell R123123 ASTM D785
Tensile Strength, Ultimate148 MPa21500 psi ASTM D638
Elongation at Break2.6 %2.6 % ASTM D638
Modulus of Elasticity9.65 GPa1400 ksi ASTM D638
Flexural Modulus8.27 GPa1200 ksi ASTM D790
Flexural Yield Strength210 MPa30500 psi ASTM D790
Compressive Yield Strength145 MPa21000 psi ASTM D695
Izod Impact, Unnotched6.94 J/cm13 ft-lb/in 1/8 in (3.18 mm) section; ASTM D256
Izod Impact, Notched0.961 J/cm1.8 ft-lb/in 1/8 in (3.18 mm) section; ASTM D256

Electrical Properties
Electrical Resistivity1e+016 ohm-cm1e+016 ohm-cm ASTM D257
Dielectric Constant4.24.2 1 MHz, Dry; ASTM D150
Dielectric Strength14.6 kV/mm370 V/mil S/T; ASTM D149
Dissipation Factor0.0070.007 1 MHz, Dry; ASTM D150
Arc Resistance75 sec75 sec ASTM D495

Thermal Properties
CTE, linear 68°F27 µm/m-°C15 µin/in-°F Flow Direction; ASTM D696
Thermal Conductivity0.317 W/m-K2.2 BTU-in/hr-ft²-°F Through-plane; ASTM C177
Deflection Temperature at 0.46 MPa (66 psi)221 °C430 °F ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)213 °C415 °F ASTM D648
Flammability, UL94V-0V-0 (V-0) at 1/16 in (1.59 mm); Per testing by RTP Company; ASTM D3801

Processing Properties
Processing Temperature343 - 366 °C650 - 690 °F 
Mold Temperature135 - 177 °C275 - 350 °F 
Injection Pressure68.9 - 103 MPa10000 - 15000 psi 

Descriptive Properties
ColorNatural/Black 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.