MatWeb, The Online Materials Database
RTP Company RTP 1405 N L Polyethersulfone (PES) Glass Fiber 30% - Lubricated - High Viscosity
Subcategory: Polyethersulfone; Polymer; Thermoplastic
Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Material Notes: Glass Fiber 30% - Lubricated - High Viscosity Comments: - Glass Fiber
- Lubricated
- High Viscosity
Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company.
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.59 g/cc | ASTM D792 |
| Filler Content | 30 % | |
| Water Absorption | 0.35 % | 24 hours at 23°C; ASTM D570 |
| Linear Mold Shrinkage | 0.002 cm/cm | 1/8 inch (3.18 mm) section; ASTM D955 |
| Linear Mold Shrinkage, 6.35 mm section | 0.002 cm/cm | 1/4 inch (6.35 mm) section; ASTM D955 |
Mechanical Properties |
|
| Hardness, Rockwell R | 123 | ASTM D785 |
| Tensile Strength, Ultimate | 21500 psi | ASTM D638 |
| Elongation at Break | 2.6 % | ASTM D638 |
| Modulus of Elasticity | 1400 ksi | ASTM D638 |
| Flexural Modulus | 1300 ksi | ASTM D790 |
| Flexural Yield Strength | 30500 psi | ASTM D790 |
| Compressive Yield Strength | 21000 psi | ASTM D695 |
| Izod Impact, Unnotched | 14 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
| Izod Impact, Notched | 1.8 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
Electrical Properties |
|
| Electrical Resistivity | 1e+016 ohm-cm | ASTM D257 |
| Dielectric Constant | 4.2 | 1 MHz, Dry; ASTM D150 |
| Dielectric Strength | 370 V/mil | S/T; ASTM D149 |
| Dissipation Factor | 0.007 | 1 MHz, Dry; ASTM D150 |
| Arc Resistance | 75 sec | ASTM D495 |
Thermal Properties |
|
| CTE, linear 68°F | 15 µin/in-°F | Flow Direction; ASTM D696 |
| Thermal Conductivity | 2.2 BTU-in/hr-ft²-°F | Through-plane; ASTM C177 |
| Deflection Temperature at 0.46 MPa (66 psi) | 430 °F | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 415 °F | ASTM D648 |
| Flammability, UL94 | V-0 | (V-0) at 1/16 in (1.59 mm); Per testing by RTP Company; ASTM D3801 |
Processing Properties |
|
| Processing Temperature | 650 - 690 °F | |
| Mold Temperature | 275 - 350 °F | |
| Injection Pressure | 10000 - 15000 psi | |
Descriptive Properties | |
| Color | Natural/Black | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |