MatWeb, The Online Materials Database
RTP Company RTP 1400 R-4300 UV Polyethersulfone (PES) PC Alloy - UV Stable
Subcategory: Polyethersulfone; Polymer; Thermoplastic
Close Analogs: Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Material Notes: PC Alloy - UV Stable Comments: Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties. Information provided by RTP Company.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
Linear Mold Shrinkage | 0.0065 cm/cm | 0.0065 in/in | 1/8 inch (3.18 mm) section; ASTM D955 |
Mechanical Properties |
|
Tensile Strength, Ultimate | 76.5 MPa | 11100 psi | ASTM D638 |
Elongation at Break | Min 10 % | Min 10 % | ASTM D638 |
Modulus of Elasticity | 2.62 GPa | 380 ksi | ASTM D638 |
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Flexural Yield Strength | 114 MPa | 16500 psi | ASTM D790 |
Izod Impact, Unnotched | 18.2 J/cm | 34 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
Izod Impact, Notched | 2.14 J/cm | 4 ft-lb/in | 1/8 in (3.18 mm) section; ASTM D256 |
Electrical Properties |
|
Electrical Resistivity | 1e+015 ohm-cm | 1e+015 ohm-cm | ASTM D257 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 182 °C | 360 °F | ASTM D648 |
Processing Properties |
|
Processing Temperature | 343 - 366 °C | 650 - 690 °F | |
Mold Temperature | 135 - 177 °C | 275 - 350 °F | |
Injection Pressure | 68.9 - 103 MPa | 10000 - 15000 psi | |
Descriptive Properties | |
Color | Natural/Black | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|