MatWeb, The Online Materials Database

RTP Company RTP 1400 R-4300 UV Polyethersulfone (PES) PC Alloy - UV Stable


Subcategory: Polyethersulfone; Polymer; Thermoplastic

Close Analogs:
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Material Notes:
PC Alloy - UV Stable

Comments:

  • PC Alloy
  • UV Stabilized

Unless otherwise specified, all data listed is for natural or black colored materials. Pigments can affect properties.

Information provided by RTP Company.

Physical PropertiesOriginal ValueComments
Specific Gravity1.32 g/cc ASTM D792
Linear Mold Shrinkage0.0065 cm/cm 1/8 inch (3.18 mm) section; ASTM D955

Mechanical Properties
Tensile Strength, Ultimate11100 psi ASTM D638
Elongation at BreakMin 10 % ASTM D638
Modulus of Elasticity380 ksi ASTM D638
Flexural Modulus380 ksi ASTM D790
Flexural Yield Strength16500 psi ASTM D790
Izod Impact, Unnotched34 ft-lb/in 1/8 in (3.18 mm) section; ASTM D256
Izod Impact, Notched4 ft-lb/in 1/8 in (3.18 mm) section; ASTM D256

Electrical Properties
Electrical Resistivity1e+015 ohm-cm ASTM D257

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)360 °F ASTM D648

Processing Properties
Processing Temperature650 - 690 °F 
Mold Temperature275 - 350 °F 
Injection Pressure10000 - 15000 psi 

Descriptive Properties
ColorNatural/Black 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.