BASF Elastollan® S98A Polyester Type Polyurethane Elastomer


Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic

Key Words: TPU Rubbers

Material Notes:
Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solvent resistance. These products can be injection and blow molded and extruded.

As with all TPU products this grade must be dried prior to processing.

Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.

Physical PropertiesOriginal ValueComments
Density1.24 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A98 ASTM D2240
Hardness, Shore D54 ASTM D2240
Tensile Strength, Ultimate42 MPa ASTM D412
Tensile Strength, Yield19 MPa Tensile stress at 100% elongation.; ASTM D-412
Tensile Strength, Yield32 MPa Tensile stress at 300% elongation.; ASTM D-412
Elongation at Break425 % ASTM D412
Tear Strength180 kN/m ASTM D624
Taber Abrasion, mg/1000 Cycles70 H-18 wheel; ASTM D-1044.
Tensile Set80 % at break; ASTM D-412

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.