BASF Elastollan® S64D Polyester Type Polyurethane Elastomer


Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic

Key Words: TPU Rubbers

Material Notes:
Recommended for injection molding. Elastollan S series of products are polyester-based thermoplastic polyurethanes that exhibit good hydrolytic stability. They also exhibit good oil, fuel and solvent resistance. These products can be injection and blow molded and extruded.

As with all TPU products this grade must be dried prior to processing.

Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.

Physical PropertiesOriginal ValueComments
Density1.25 g/cc ASTM D792

Mechanical Properties
Hardness, Shore D64 ASTM D2240
Tensile Strength, Ultimate39 MPa ASTM D412
Tensile Strength, Yield27 MPa Tensile stress at 100% elongation.; ASTM D-412
Tensile Strength, Yield37 MPa Tensile stress at 300% elongation.; ASTM D-412
Elongation at Break380 % ASTM D412
Tear Strength220 kN/m ASTM D624
Taber Abrasion, mg/1000 Cycles50 H-18 wheel; ASTM D-1044.
Tensile Set135 % at break; ASTM D-412

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.