MatWeb, The Online Materials Database

BASF Elastollan® C-78A Polyester Type Polyurethane Elastomer


Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic

Key Words: TPU Rubbers

Material Notes:
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fuel and solvent resistance. These products can be injection and blow molded and extruded.

As with all TPU products this grade must be dried prior to processing.

Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.

Physical PropertiesMetricEnglishComments
Density1.18 g/cc0.0426 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore A8080 ASTM D2240
Tensile Strength, Ultimate37 MPa5370 psi ASTM D412
Tensile Strength, Yield1.1 MPa160 psi Tensile stress at 300% elongation.; ASTM D-412
Tensile Strength, Yield5.2 MPa754 psi Tensile stress at 100% elongation.; ASTM D-412
Elongation at Break690 %690 % ASTM D412
Tear Strength85 kN/m485 pli ASTM D624
Taber Abrasion, mg/1000 Cycles2525 H-18 wheel; ASTM D-1044.
Tensile Set25 %25 % at break; ASTM D-412

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.