MatWeb, The Online Materials Database

BASF Elastollan® C-80A Polyester Type Polyurethane Elastomer


Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic

Key Words: TPU Rubbers

Material Notes:
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fuel and solvent resistance. These products can be injection and blow molded and extruded.

As with all TPU products this grade must be dried prior to processing.

Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.

Physical PropertiesOriginal ValueComments
Density1.19 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A82 ASTM D2240
Tensile Strength, Ultimate36 MPa ASTM D412
Tensile Strength, Yield1.1 MPa Tensile stress at 300% elongation.; ASTM D-412
Tensile Strength, Yield5.5 MPa Tensile stress at 100% elongation.; ASTM D-412
Elongation at Break700 % ASTM D412
Tear Strength85 kN/m ASTM D624
Taber Abrasion, mg/1000 Cycles25 H-18 wheel; ASTM D-1044.
Tensile Set30 % at break; ASTM D-412

Electrical Properties
Electrical ResistivityMin 1e+010 ohm-cm DIN 53482/VDE 0303
Surface ResistanceMin 1e+010 ohm DIN 53482/VDE 0303
Dielectric Constant6.1 1 MHz; DIN 53483/VDE 0303
Dielectric Constant6.6 1 kHz; DIN 53483/VDE 0303
Dielectric Constant, Low Frequency7.1 at 50 Hz; DIN 53483/VDE 0303
Dielectric Strength31 kV/mm DIN 53481/VDE 0303
Dissipation Factor0.024 1 kHz
Dissipation Factor0.053 1 MHz
Dissipation Factor, Low Frequency0.2 50 Hz
Comparative Tracking IndexMin 600 V DIN/IRC 112

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.