MatWeb, The Online Materials Database

BASF Elastollan® C-90A Polyester Type Polyurethane Elastomer


Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic

Key Words: TPU Rubbers

Material Notes:
Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fuel and solvent resistance. These products can be injection and blow molded and extruded.

As with all TPU products this grade must be dried prior to processing.

Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.

Physical PropertiesOriginal ValueComments
Density1.21 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A93 ASTM D2240
Hardness, Shore D41 ASTM D2240
Tensile Strength, Ultimate41 MPa ASTM D412
Tensile Strength, Yield10 MPa Tensile stress at 100% elongation.; ASTM D-412
Tensile Strength, Yield22 MPa Tensile stress at 300% elongation.; ASTM D-412
Elongation at Break550 % ASTM D412
Tear Strength120 kN/m ASTM D624
Taber Abrasion, mg/1000 Cycles25 H-18 wheel; ASTM D-1044.
Tensile Set50 % at break; ASTM D-412

Electrical Properties
Comparative Tracking IndexMin 600 V DIN/IRC 112

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.