BASF Elastollan® C-64D Polyester Type Polyurethane Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU Rubbers
Material Notes: Recommended for injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellent oil, fuel and solvent resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing. Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Physical Properties | Original Value | Comments |
|
Density | 1.24 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 64 | ASTM D2240 |
Tensile Strength, Ultimate | 40 MPa | ASTM D412 |
Tensile Strength, Yield | 26 MPa | Tensile stress at 100% elongation.; ASTM D-412 |
Tensile Strength, Yield | 38 MPa | Tensile stress at 300% elongation.; ASTM D-412 |
Elongation at Break | 430 % | ASTM D412 |
Modulus of Elasticity | 0.4 GPa | |
Shear Modulus | 0.25 GPa | |
Tear Strength | 220 kN/m | ASTM D624 |
Taber Abrasion, mg/1000 Cycles | 50 | H-18 wheel; ASTM D-1044. |
Tensile Set | 100 % | at break; ASTM D-412 |
Electrical Properties |
|
Electrical Resistivity | Min 1e+013 ohm-cm | DIN 53482/VDE 0303 |
Surface Resistance | Min 1e+012 ohm | DIN 53482/VDE 0303 |
Dielectric Constant | 4.1 | 1 MHz; DIN 53483/VDE 0303 |
Dielectric Constant | 4.8 | 1 kHz; DIN 53483/VDE 0303 |
Dielectric Constant, Low Frequency | 5.1 | at 50 Hz; DIN 53483/VDE 0303 |
Dielectric Strength | Min 49 kV/mm | DIN 53481/VDE 0303 |
Dissipation Factor | 0.031 | 1 kHz |
Dissipation Factor | 0.045 | 1 MHz |
Dissipation Factor, Low Frequency | 0.034 | 50 Hz |
Comparative Tracking Index | Min 600 V | DIN/IRC 112 |
Thermal Properties |
|
Vicat Softening Point | 165 °C | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|