MatWeb, The Online Materials Database

BASF Elastollan® 1175AW Polyether Type Polyurethane Elastomer


Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic

Key Words: TPU Rubbers

Material Notes:
Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhibit excellent low temperature properties, hydrolysis resistance and fungus resistance. These products can be injection and blow molded and extruded.

As with all TPU products this grade must be dried prior to processing.

Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.

Physical PropertiesOriginal ValueComments
Density1.14 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A76 ASTM D2240
Tensile Strength, Ultimate30 MPa ASTM D412
Tensile Strength, Yield4.3 MPa Tensile stress at 100% elongation.; ASTM D-412
Tensile Strength, Yield8.3 MPa Tensile stress at 300% elongation.; ASTM D-412
Elongation at Break740 % ASTM D412
Tear Strength80 kN/m ASTM D624

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.