MatWeb, The Online Materials Database
BASF Elastollan® 1180A Polyether Type Polyurethane Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU Rubbers
Material Notes: Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhibit excellent low temperature properties, hydrolysis resistance and fungus resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing. Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
| Physical Properties | Original Value | Comments |
|
| Density | 1.11 g/cc | ASTM D792 |
Mechanical Properties |
|
| Hardness, Shore A | 80 | ASTM D2240 |
| Tensile Strength, Ultimate | 32 MPa | ASTM D412 |
| Tensile Strength, Yield | 10 MPa | Tensile stress at 300% elongation.; ASTM D-412 |
| Tensile Strength, Yield | 5.5 MPa | Tensile stress at 100% elongation.; ASTM D-412 |
| Elongation at Break | 600 % | ASTM D412 |
| Tear Strength | 90 kN/m | ASTM D624 |
| Taber Abrasion, mg/1000 Cycles | 25 | H-18 wheel; ASTM D-1044. |
| Tensile Set | 45 % | at break; ASTM D-412 |
Electrical Properties |
|
| Electrical Resistivity | Min 1e+011 ohm-cm | DIN 53482/VDE 0303 |
| Surface Resistance | Min 1e+011 ohm | DIN 53482/VDE 0303 |
| Dielectric Constant | 6.5 | 1 MHz; DIN 53483/VDE 0303 |
| Dielectric Constant | 7.6 | 1 kHz; DIN 53483/VDE 0303 |
| Dielectric Constant, Low Frequency | 8 | at 50 Hz; DIN 53483/VDE 0303 |
| Dielectric Strength | 39 kV/mm | DIN 53481/VDE 0303 |
| Dissipation Factor | 0.026 | 1 kHz |
| Dissipation Factor | 0.087 | 1 MHz |
| Dissipation Factor, Low Frequency | 0.121 | 50 Hz |
| Comparative Tracking Index | Min 600 V | DIN/IRC 112 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |