BASF Elastollan® 1174D Polyether Type Polyurethane Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU Rubbers
Material Notes: Recommended for injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes. They exhibit excellent low temperature properties, hydrolysis resistance and fungus resistance. These products can be injection and blow molded and extruded. As with all TPU products this grade must be dried prior to processing. Property values below are typical values based on test samples cured 20 hours at 100°C before testing. Information provided by BASF Corporation.
Physical Properties | Metric | English | Comments |
|
Density | 1.19 g/cc | 0.043 lb/in³ | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 73 | 73 | ASTM D2240 |
Tensile Strength, Ultimate | 45 MPa | 6530 psi | ASTM D412 |
Tensile Strength, Yield | 32 MPa | 4640 psi | Tensile stress at 100% elongation.; ASTM D-412 |
Tensile Strength, Yield | 38 MPa | 5510 psi | Tensile stress at 300% elongation.; ASTM D-412 |
Elongation at Break | 350 % | 350 % | ASTM D412 |
Tear Strength | 255 kN/m | 1460 pli | ASTM D624 |
Taber Abrasion, mg/1000 Cycles | 75 | 75 | H-18 wheel; ASTM D-1044. |
Tensile Set | 80 % | 80 % | at break; ASTM D-412 |
Electrical Properties |
|
Electrical Resistivity | Min 1e+012 ohm-cm | Min 1e+012 ohm-cm | DIN 53482/VDE 0303 |
Surface Resistance | Min 1e+012 ohm | Min 1e+012 ohm | DIN 53482/VDE 0303 |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|