BASF Elastollan® 1175A10W Wire & Cable Grade Polyurethane Elastomer
Subcategory: Elastomer, TPE; Polymer; Polyurethane, TP; Thermoplastic
Key Words: TPU Rubbers
Material Notes: As with all TPU products this grade must be dried prior to processing. Information provided by BASF Corporation.
Physical Properties | Original Value | Comments |
|
Density | 1.14 g/cc | 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C.; ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 75 | 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C.; ASTM D2240 |
Tensile Strength, Ultimate | 41 MPa | 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C; ASTM D412 |
Tensile Strength, Yield | 11 MPa | Tensile stress at 300% elongation; 0.76 mm (0.030 in) extruded sheet; ASTM D-412 |
Tensile Strength, Yield | 4.8 MPa | Tensile stress at 100% elongation.; ASTM D-412 |
Elongation at Break | 685 % | on 0.030 in extruded sheet; ASTM D-412 |
Flexural Modulus | 0.025 GPa | 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C.; ASTM D790 |
Tear Strength | 27 kN/m | Split tear strength (ASTM D-1938) on 0.76 mm ( 0.030 inch) extruded sheet |
Graves Tear Strength | 57 kN/m | on 0.76 mm ( 0.030 inch) extruded sheet; ASTM D624 |
Taber Abrasion, mg/1000 Cycles | 20 | H-18 wheel; ASTM D-1044; 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C. |
Compression Set | 25 % | 22 hr at 23°C per ASTM D-395; 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C. |
Compression Set, Elevated Temperature | 45 % | 22 hr @ 70°C; ASTM D-395; 0.080 in molded plaque after curing 20 hrs at 100°C. |
Tensile Set | 32 % | at 200% elongation per ASTM D-412 is on 0.030 in extruded sheet. |
Thermal Properties |
|
Vicat Softening Point | 80 °C | 2.0 mm (0.080 in) molded plaque, cured 20 hr at 100°C.; ASTM D1525 |
Glass Temperature | -47 °C | Pellet sample |
Flammability, UL94 | V-2 | Color: NC; 1.59 mm |
Flammability, UL94 | V-2 | Color: NC; 3.14 mm |
Flammability, UL94 | V-0 | Color: NC; 0.9 mm |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|