Texaco Multigear® EP SAE 80W-90


Subcategory: Fluid; Lubricant

Close Analogs: CPS Number: 222316; MSDS Number: 8628

Material Notes:
Texaco Multigear EP oils deliver value through:

  • Improved durability — Specially formulated to stand up to the demands of severe service applications.
  • Extended gear life — Extreme pressure properties protect hypoid and other types of gears from scuffing and wear under heavily loaded conditions.
  • Long lubricant life — Outstanding thermal and oxidation stability allow high temperature operation with long lubricant life without the formation of sludge and deposits.
  • All-weather protection — Multiviscosity characteristics assure proper gear lubrication at both low and high ambient temperatures.
  • Corrosion and rust protection — Effective inhibitor package prevents rusting or corrosion of gears and bearings surfaces.

Texaco Multigear EP oils are multipurpose lubricants.

They are made with:

  • Highly refined base stocks
  • A carefully balanced additive package to provide maximum gear protection, long lubricant life and excellent field performance
  • Sulfur-phosphorus extreme pressure additives that provide superior thermal and oxidation stability
  • Rust and corrosion inhibitors, a foam inhibitor, and a pour point depressant

The highly refined base stocks and various inhibitors in the additive package assure a well-balanced lubricant and long gear and bearing life with maximum durability.

Texaco Multigear EP oils are recommended for use in all spiral bevel and hypoid differentials, power dividers, and oil-lubricated steering axle wheel bearings.

They are designed for complete refill and make-up of all passenger car, light duty and heavy duty truck transmissions, conventional differentials and steering gears.

Their multiviscosity characteristics allow their use in equipment operating over a broad ambient temperature range. This means good cold flow properties and gear protection.

Texaco Multigear EP oils meet the performance requirements of:

  • API Service Categories MT-1, GL-4, and GL-5
  • Are qualified for SAE J 2360 (formerly known as MIL-PRF-2105E)

They also meet the requirements of:
  • A Mack GO-J fluid
  • Rockwell 0-76D (SAE 80W-90), 0-76-A (SAE 85W-140)

Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing.

Physical PropertiesOriginal ValueComments
API Gravity28.4 ° 
Brookfield Viscosity118000 cP -26°C
Viscosity Measurement95 Viscosity Index
Saybolt Viscosity at 100°F762 SUS 
Saybolt Viscosity at 210°F76.4 SUS 
Kinematic Viscosity at 40°C (104°F)145 cSt 
Kinematic Viscosity at 100°C (212°F)14.2 cSt 

Thermal Properties
Pour Point-33 °C 
Flash Point221 °C 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.