Zirconium Oxide Ceramic Zirconia,Tetragonal, Y2O3 Stabilized

 

Subcategory: Oxide, Zirconium; Oxide

Key Words: ZrO2; YSZ

Material Notes:
Data provided by the supplier, MarkeTech International.

Zirconium oxide is widely used and has superior high temperature properties. When combined with yttria the strength and fracture toughness is significantly improved. This makes some grades of zirconia superior to most materials for abrasion and wear resistance. Parts can be machined before firing in the green state and after firing to meet exacting specifications. Zirconia is electrically conductive above 900°C. Zirconia can be tape cast into very thin sheets for fuel cells and engineered ceramics.

Available Properties
  • Density
  • Knoop Microhardness
  • Modulus of Elasticity
  • Flexural Strength
  • Compressive Yield Strength
  • CTE, linear 20°C
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。