Silica Aerogel

 

Subcategory: Aerogel; Oxide, Silicon; Oxide

Close Analogs: Resorcinol Formaldehyde and Carbon Aerogels are also listed in MatWeb.

Key Words: Silica Aerogels; MarkeTech International; SiO2; Silicon Oxide; Silicon Dioxide

Material Notes:
Silica Aerogels are generally known for being an extremely lightweight transparent solid (down to <0.05 g/cm3 with excellent thermal insulating properties, high temperature stability, very low dielectric constant, and extremely high surface area. Some initial applications have included atomic particle detectors and super insulation for aerospace applications and they were used to insulate the Mars rover.

MarkeTech International standard silica aerogel is formed into translucent monolithic blocks with carefully controlled densities. The standard density is nominally 0.1 g/cm3 with a surface area of about 800 m2/g. Densities from 0.01 to 0.30 g/cm3 are commonly available.

Data provided by the supplier, MarkeTech International.

Available Properties
  • Density
  • Particle Size
  • Specific Surface Area
  • Tensile Strength, Ultimate
  • Modulus of Elasticity
  • Compressive Modulus
  • Poissons Ratio
  • Fracture Toughness
  • Electrical Resistivity
  • Dielectric Constant
  • CTE, linear 20°C
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Refractive Index
  • Color
  • Mean Pore Diameter
  • Solids
  • Sound Velocity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。