GE Advanced Ceramics AC6069 Boron Nitride (BN) Powder

 

Subcategory: Nitride; Additive/Filler for Polymer

Material Notes:
GE Advanced Ceramics boron nitride (BN) powder grade AC6069 consists of single-crystal hexagonal particles with an average particle size of 9 µm. AC6069 has a relatively tight particle size distribution, and over 99% of the particles pass through a 325 mesh. The single-crystal nature of AC6069 powder gives it outstanding lubrication properties, and its fineness helps it disperse well in a wide range of media.

Applications:

AC6069 is commonly used as a release agent and lubricantfor high-temperature glass making and metalforming processes. Additionally, its small size and good dispersion properties make it a good nucleation additive for plastics foaming or solidification.

AC6069 is also suitable in the broad range of applications for which boron nitride is well-suited – thermal management materials, refractory coatings, hot-pressed solids and composites, etc.

GE Advanced Ceramics produces over 75 standard and custom grades of BN powders to meet a wide range of application requirements, and has over 40 years of expertise in the synthesis and refinement of boron nitride powders.

Information provided by GE Advanced Ceramics.

Available Properties
  • Density
  • Particle Size
  • Specific Surface Area
  • Carbon
  • Color
  • Crystal Type
  • Oxygen
  • Sol. Borate
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。