GE Advanced Ceramics HBR Hot-Pressed Boron Nitride

 

Subcategory: Nitride

Key Words: BN

Material Notes:
Hot-pressed BN is compacted at temperatures up to 2000°C and pressures up to 2000 psi to form a dense, strong engineering material that is easily machined. It is available in standard and custom hot-pressed shapes and has several unique characteristics and physical properties which make it valuable for solving tough problems in a wide range of industrial applications.

Four Material Grades HBC and HBT are the highest purity hot-pressed boron nitrides commercially available. They are diffusion bonded and feature a low dielectric constant, minimal moisture pick-up, and low loss tangent which makes them ideal for electronic applications. Grade HBT, although lower in strength and density than HBC, is available in larger sizes, at lower cost, and usually with a shorter delivery schedule. Grade HBN uses small amounts of boric oxide as a binder and should be used in applications where hydration and thermal shock are not a concern. Grade HBR uses calcium borate as a binder and is less sensitive to moisture.

Thermal Management The unique combination of being both an excellent electrical insulator and thermal conductor makes BN very useful as a heat sink in high power electronic applications. Its properties compare favorably with beryllium oxide, aluminum oxide and other electronic packaging materials, yet is easier to form and finish.

High Temperature Applications Temperature stability and excellent resistance to thermal shock makes BN the material of choice in the toughest high temperature applications such as equipment for plasma arc welding, diffusion source wafers, and semiconductor crystal growth equipment & processing.

Molten Metal HandlingBN is inorganic, inert, nonreactive with halide salts and reagents, and is not wet by most molten metals and slags. These characteristics, combined with low thermal expansion, make it ideal for interface materials used in various molten metal processes.

Information provided by GE Advanced Ceramics.

Available Properties
  • Density
  • Binder Melting Point
  • Water Absorption
  • Open Porosity
  • Hardness, Knoop
  • Modulus of Elasticity
  • Flexural Strength
  • Compressive Yield Strength
  • Electrical Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • Dissipation Factor
  • CTE, linear 1000°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Maximum Service Temperature, Inert
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。