Astro Met, Inc. AmAlOx 68 Alumina - Aluminum Oxide

 

Subcategory: Oxide, Aluminum; Oxide

Material Notes:
General Description:

AmAlOx 68 alumina (Astro Met Aluminum Oxide) is a high purity 99.8% aluminum oxide (alumina) ceramic which has been developed and optimized for maximum wear resistance and corrosion resistance. A high density, diamond like hardness, fine grain structure and superior mechanical strength are the unique properties that make AmAlOx 68 alumina the material of choice for a wide range of demanding applications. AmAlOx 68 alumina provides a cost-effective, engineered material solution in applications that require the optimum in wear resistance, corrosion resistance, high temperature stability, low thermal expansion, high stiffness to weight ratio, high dielectric strength and biocompatibility.

Available Properties
  • Bulk Density
  • Water Absorption
  • Particle Size
  • Hardness, Vickers
  • Modulus of Elasticity
  • Flexural Strength
  • Poissons Ratio
  • Fracture Toughness
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Color
  • Gas Permeation, %
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。