Dicronite® Tungsten Disulfide Dry Lubricant

 

Subcategory: Sulfide/Chalcogenide; Ceramic/Metallic Coating

Key Words: WS2, Dicronite® Dry Lube

Material Notes:
Dicronite® is an extensively modified lamellar composition of Tungsten Disulfide. It molecularly bonds to most materials and platings. Dicronite® transmigrates into the molecular structure of the substrate and can only be eliminated by removing the bonded substrate.

Industrial applications: Mold operation, mold release, lubricity (can be applied to similar or non-similar substrates to prevent wear, galling and seizing. Applied at ambient temperature and with twice the lubricity of graphite), medical, ball and roller bearings, linear bearings, ball screws, pumps, compressors, and blowers.

Carrier - Dry air, no binders or adhesives. No cure time required, applied at ambient temperature. Inert, non-toxic, corrosion resistant. Accepts most paints and is compatible with most solvents, fuels and oils. Insensitive to detonation by or in the presence of oxygen. Will not cause distortive stress relief, additional stresses or degradation to any surface. Approvals - NAMSA class 6 (medical) and USDA; ISO-10993 medically approved .

Information provided by Dicronite.

Available Properties
  • Density
  • Molecular Weight
  • Thickness
  • Hardness, Mohs
  • Compressive Strength
  • Coefficient of Friction
  • Maximum Service Temperature, Air
  • Maximum Service Temperature, Inert
  • Minimum Service Temperature, Air
  • Color
  • Magnetism
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。