Goodfellow Leachable Ceramic (Silica, Zircon, Alumina)

 

Subcategory: Oxide, Silicon

Material Notes:
SiO2 50/ZrSiO4 40/Al2O3 10

General Description:

This form of ceramic is used in the precision foundry industry. The tubes and rods are incorporated into moulds in the lost wax process. Using this technique, very fine tolerances on diameter can be obtained. The ceramic is leached away by the using sodium hydroxide solution once the metal has solidified. This leachable ceramic has a high porosity, does not have an organic binder, but does absorb water.

Information provided by Goodfellow.

Available Properties
  • Density
  • Water Absorption at Saturation
  • Porosity
  • CTE, linear 20°C
  • CTE, linear 1000°C
  • Maximum Service Temperature, Air
  • Chemical Resistance - Alkalis
  • Chemical Resistance - Concentrated Acids
  • Chemical Resistance - Dilute Acids
  • Chemical Resistance - Halogens
  • Chemical Resistance - Metals
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。