Goodfellow Tungsten Carbide/Cobalt

 

Subcategory: Metal Matrix Composite; Carbide

Material Notes:
General Description

Tungsten Carbide is a hard, brittle ceramic which, when combined with 6% to 10% Cobalt, forms a tough Cermet (Ceramic-Metal). This material was developed for use in cutting tools, having hard ceramic crystals of a few microns in size within a ductile metal matrix. The resulting material can withstand the high compressive stresses imposed during cutting, as well as having good wear and oxidation resistance at the high temperatures reached. Tungsten Carbide/ Cobalt has a high resistance to thermal shock, so is able to withstand the rapid temperature fluctuations. Also, this has found a use as electrodes for Electrode Discharge Machining.

Information provided by Goodfellow.

Available Properties
  • Density
  • Vickers Microhardness
  • Tensile Strength at Break
  • Tensile Modulus
  • Compressive Strength
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 1000°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。