Mid-Mountain Materials Thermoseal® P120 Thermal Coating

 

Subcategory: Ceramic/Metallic Coating; Ceramic

Material Notes:
Description: A family of high temperature resistant coatings which may be applied by busing, rolling, dipping, or spraying. Used on materials which require surface hardening to protect against flame erosion, molten metal corrosion and thermal spalling.

APPLICATION: Mix well before using. Surfaces to be coated or treated should be cleaned and roughened prior to application for best adhesion. The mix and the substrate should be between 60ºF • 15ºC and 80ºF •27ºC for best results. Dry each coat, either in air or with an external heat source prior to applying additional coats if desired. Firing above 1600ºF • 879ºC will create ceramic bonding in the coating to increase it's strength in the P-series materials.

USES:

  • Cement or adhering ceramic fiber paper to substrates
  • Coatings for furnaces, troughs, burners, molds
  • Protective coating for hose and cable covering
  • Induction furnace coil coating
  • Molten metal splash protection

PACKAGING: THERMOSEAL® THERMAL COATINGS are available in one gallon cans, (four cans per case) in five gallon plastic buckets, and in 55 gallon drums. Do NOT allow to freeze.

Information provided by Mid-Mountain Materials.

Available Properties
  • Solids Content
  • Thickness
  • Maximum Service Temperature, Air
  • Appearance
  • Color
  • Composition
  • Coverage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。