3M Nextel™ 650 Composite Ceramic Fiber

 

Subcategory: Oxide, Zirconium; Oxide, Aluminum; Oxide; Composite Fibers

Close Analogs: This grade is not a current part of the 3M product line.

Key Words: Alumina, Aluminum Oxide

Material Notes:
Chemical composition above is wt%. Crystal phases are alpha alumina + yttria stabilized zirconia. Filament diameter is 10-12 µm.

3M Nextel Ceramic Fibers 610, 650, and 720 are composite grade fibers. They have a refined crystal structure based on alpha-Al2O3 and do not contain glassy phases. This allows the fibers to retain their strength at high temperatures. 3M Nextel Fiber 650, an alpha-Al2O3 with Y2O3 and ZrO2 additions, has improved strength retention at temperature due to reduced grain boundary sliding. The Y2O3 and ZrO2 additions also help to 'pin' the grains and reduce grain growth when exposed to thermal aging.

Information provided by 3M Ceramic Textile and Composites.

Available Properties
  • Density
  • Particle Size
  • Specific Surface Area
  • Tensile Strength, Ultimate
  • Modulus of Elasticity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Melting Point
  • Refractive Index
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。