Pyrotek SF-50 Foamed Fused Silica Insulation Board

 

Subcategory: Oxide, Silicon; Oxide

Material Notes:
SF-50 is characterized by its uniform open cell structure which allows it to be machined to close tolerances. It can be drilled, sawed or modified with conventional tools. For quick construction of structures, SF-50 is easily joined together with Pyrotek's FSC-2000 fused silica cement. SF-50 has excellent volume stability which allows for its use in severe cyclic conditions. Additionally, the absence of any flux or other impurities allows for its use in chemically critical applications.

Applications

  • Back-up thermal insulation
  • Furnace door, roof and siding
  • Wall lining
  • Vessel liners
  • Aluminum trough liners
  • Reflectors for quartz lamps and infra-red heaters
  • Heat treating and dies
  • Tooling fixtures
  • Incinerators
  • Brazing fixtures
  • Gas take-up liners
  • Thermal barriers
  • Nuclear applications

Advantages

  • Exceptional thermal insulation properties
  • Exceptional resistance to thermal shock
  • Volume stability over a wide temperature range
  • Excellent dielectric strength
  • Ease of shaping provides freedom in engineering design and ease of construction

Information provided by Pyrotek.

Available Properties
  • Density
  • Water Absorption
  • Modulus of Rupture
  • Compressive Strength
  • Thermal Conductivity at Elevated Temperature
  • Maximum Service Temperature, Air
  • Shrinkage
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。