SAES Getters Nd:YAG Solid State Laser Crystals (Nd-doped Y3Al5O12)

 

Subcategory: Oxide, Aluminum

Key Words: Neodymium YAG (Yttrium Aluminum Garnet Y3Al5O12)

Material Notes:
Y3-xNdxAl5O12 where Nd doping level between 0.2 and 1.4% atomic. Among solid-state laser crystals, Nd:YAG is the most versatile and suitable for a wide range of applications due to its physical properties, low threshold, high gain and narrow linewidth. Typical applications include the military, medicine and material processing industries for cutting, welding, drilling, marking and repairing. Nd:YAG lasers are also employed in application areas characterized by harsh enviromental conditions, like remote sensing, ocean and atmospheric experiments. Ultrapure gas and superior raw material purity, together with a tightly controlled proprietary process, allow us to proudly offer premium grade Nd:YAG crystal rods with low losses and superior efficiency.

Nd concentration uniformity along each rod is achieved by using only a small portion (about 20%) of the melt. A very uniform Nd profile is certified for each boule, that is also marked with laser for identification.

Information provided by SAES Getters.

Available Properties
  • Density
  • a Lattice Constant
  • Molecular Weight
  • Hardness, Mohs
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Refractive Index
  • Crystal Structure
  • Lasing Wavelength
  • Primary Diode Pump Band
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。