SPHERE ONE EXTENDOSPHERES™ PM 6550 Hollow Spheres

 

Subcategory: Additive/Filler for Polymer; Thermoplastic

Material Notes:
PM 6550 PM 6550 is an extremely light and versatile hollow sphere. Its plastic composition results in a very low density product. Only a very small amount of this hollow sphere is needed to provide substantial volume filling in formulations. PM 6550 has excellent flexibility, and the walls of the hollow sphere can survive a variety of stress environments. PM 6550 offers good resistance to solvents. The oleophilic surface permits easy dispersion in organic fluids and resins, but also provides good wet-out in latex systems.

Applications: PM 6550 can be used to cover the whole range of applications where Sphere One hollow spheres would be incorporated. Plastic hollow spheres have found utility in such wide ranging applications as emulsion explosives, autobody putties, sealants and epoxy syntactic foams.

Information provided by Sphere One Inc.

Available Properties
  • Density
  • Bulk Density
  • Particle Size
  • Maximum Service Temperature, Air
  • Color
  • Physical Form
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。