Saint-Gobain Spectrosil® 2200 Optical Fused Quartz

 

Subcategory: Glass; Oxide, Silicon; Oxide

Material Notes:
Spectrosil® 2200 grade is an excimer laser grade developed for maximum transmission and prolonged life in microlithography and other critical deep UV applications using KrF (248 nm) and ArF (193 nm) excimer lasers.

Spectrosil® is a synthetic fused silica manufactured using a patented, environmentally friendly process that results in a virtually chlorine-free material of exceptional purity which is bubble-free and fluorescence-free. The 2000 series has excellent optical transmission from 180 nm in the deep UV through to 2000 nm in the IR Available in ingot, rod, tube, and components.

General properties of Fused Silica and Fused quartz: A very wide transmission range from UV to near IR; extremely high optical transmission, excellent resistance to high power laser energy, excellent homogeneity, high temperature resistance, very low thermal expansion (resistance to thermal shock), and chemical inertness. General uses for optical quartz are microlithography optical systems, optical fibers, photomasks, laser optics, LCD displays, light guides, optical, IR , and UV windows, spectrophotometer cells, slides, optical pyrometers, and lamp bodies/components.

Information provided by Saint-Gobain Quartz PLC.

Available Properties
  • Density
  • Hardness, Knoop
  • Vickers Microhardness
  • Hardness, Mohs
  • Modulus of Elasticity
  • Flexural Strength
  • Compressive Yield Strength
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity at Elevated Temperature
  • Dielectric Constant
  • Dissipation Factor
  • CTE, linear 20°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Softening Point
  • Annealing Point
  • Strain Point
  • Refractive Index
  • Transmission, Visible
  • IR Transmittance
  • UV Transmittance
  • Bubble Class
  • Bubbles; Sum of CSA
  • Inclusions
  • Refractive Index Homogeneity
  • Residual Strain
  • Striae
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。