Thermal Ceramics Cerablanket Blanket

 

Subcategory: Oxide

Material Notes:
Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on average the highest tensile strength of any Thermal Ceramics ceramic fiber blanket. Cerablanket is available in a wide variety of densities and sizes. Cerablanket offers excellent handleability and high temperature stability which allows it to meet a wide range of hot face and back up insulation applications in furnaces, kilns and other equipment requiring high temperature heat containment.

Military Specifications and Approvals:

  • Mil-I-23128A- 3, 6 pcf blanket
  • Mil-I-24244- all blankets
  • Mil-I-23128B- 6, 8 pcf blanket
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Thickness
    • Thermal Conductivity at Elevated Temperature
    • Melting Point
    • Maximum Service Temperature, Air
    • Other Element Content
    • Water Leachable Elements on Surface of Fiber, PPM
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。