Thermal Ceramics TR-20 Block Insulation

 

Material Notes:
TR-20 Block is a superior, high-temperature insulation for service to 2000°F (1095°C). According to ASTM testing procedures, TR-20 exhibits extremely high resistance to breakage to 2000°F (1095°C). Long, maintenance-free service and maximum operating efficiency is assured by TR-20’s unique combination of low conductivity and high stability. TR-20 is also very low in sulfur and iron, making it highly resistant to attack from atmospheric conditions and greatly reducing the possibility of product contamination.

These products can be manufactured in special shapes to fit.

Features:

  • Low thermal conductivity
  • Block construction 36" x 12"
  • Good high temperature strength
  • Variety of thicknesses up to 7”
  • Resistant to cryolite vapors

    Applications:

  • Side and end wall insulating material in carbon baking pits
  • Backup insulation in aluminum pot cells, reheat and pusher furnaces, copper reverberatory furnaces, and oil-fired water tube boilers

    Curved Block

  • Interior and exterior use on bustle pipes, hot air pipes, stacks and other curved or circular equipment
  • customer specifications, saving money on both installation and energy costs.

    Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Loss On Ignition
    • Porosity
    • Modulus of Rupture
    • Compressive Strength
    • Specific Heat Capacity
    • Thermal Conductivity at Elevated Temperature
    • Maximum Service Temperature, Air
    • Shrinkage
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。