Thermal Ceramics Kao-Plas G65 Plastic Monolithics

 

Material Notes:
Kao-Plas G65 is a 65%-alumina, guniting-plastic monolith with a use limit of 3100°F (1704°C). It is supplied as a dry powder for use in onventional guniting equipment. No prewet is used with all water for placement added at the nozzle using the same techniques used in the guniting of astables. There is no need for special equipment or extremely high air pressures for the placement of this type of guniting plastic. It possesses excellent thermal shock resistance throughout its temperature range. Kao-Plas G65 can also be troweled or hand rammed by adding 10 to 12% water to the dry mix in a mechanical mixer. It has excellent resistance to molten slag and thermal shock.

Information provided by Thermal Ceramics

Available Properties
  • Density
  • Compressive Strength
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Shrinkage
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。