Thermal Ceramics 3000M Unifelt

 

Material Notes:
Unifelt Veneering modules, 3000 (HT), 3000 M, XT are made from a blend of high-temperature Kaowool fiber and Saffil alumina fiber. The modules are fabricated into blocks, 12" by 12" (305 mm x 305 mm) using pre-cut Unifelt boards turned edge-grain and glued together.

Unifelt veneering modules are part of the Unisystem family of products. They can be applied over a variety of surfaces including refractory castable, monolithic plastics, high-temperature IFB and ceramic fiber modules. K-Bond mortar, a high-temperature air setting mortar is used to attach the Unifelt modules. Unikote S surface coating is then applied over the module hot face to provide greater thermal stability and chemical attack resistance. A typical application would be stack-on-stack design linings over new ceramic fiber weld-on modules.

Features:

  • 12" x 12" (305 mm x 305 mm) blocks of ceramic fiber insulation
  • Easily installed over existing refractory surface
  • Improves furnace efficiency without replacing a serviceable refractory lining
  • Good insulating properties
  • Excellent thermal stability
  • Applications:

  • Forge furnaces
  • Crucible furnace
  • Rotary hearth furnace
  • Holding furnace
  • Heat treating furnace
  • Pusher reheat furnace
  • Ceramic kiln
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Loss On Ignition
    • Thermal Conductivity
    • Maximum Service Temperature, Air
    • Other Element Content
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。