Thermal Ceramics Pyro-Bloc E and E2 Modules

 

Material Notes:
Pyro-Bloc E Modules are an edge-grained ceramic fiber block used for lining industrial furnaces. The E Module was designed especially for furnaces operating up to 1800°F. The E Module is manufactured from R Grade Pyro-Log fiber and comes in a 12" x 16" (305 mm x 406 mm) block from 3" to 6" (76 mm x 152 mm) thick. The 304SS internal support system features the patented one-shot Y Module attachment system. All these features make the E Module an economical alternative to ceramic fiber wall paper systems in lining lower temperature industrial furnaces. The E Module comes complete with internal support system and stud already in place.

Features:

  • Monolithic, edge-grained ceramic fiber module
  • Extremely fast, efficient installation
  • One-shot center-fired stud
  • Applications:

  • Annealing furnaces
  • Heat treating furnaces
  • Crude heaters
  • Incinerators
  • Process heaters
  • Information provided by Thermal Ceramics

    Available Properties
    • Density
    • Thermal Conductivity
    • Melting Point
    • Maximum Service Temperature, Air
    • Loss on Ignition
    • Other Element Content
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。