Thermal Ceramics Bulk FireMaster

 

Material Notes:
FireMaster Bulk is used in UL Systems CAJ1053 and CAJ3032 for pipe and cable bundle penetrations. These UL systems have been tested to ASTM E814/UL1479. For further details, refer to the UL Fire Resistance Directory, Vol. II, or contact Thermal Ceramics. The bulk is a high-temperature fiber which is classified by Underwriters Laboratories (UL) under “Loose Fill Materials (BPHX)” in the UL Building Materials Directory, No. R9464. FireMaster Bulk is used as a fireproof fill, void, or cavity material for several UL systems. It is the base fiber for FireMaster products.

Features:

  • UL-classified, noncombustible material
  • Lightweight/flexible
  • Optional foil facing or encapsulation
  • Low thermal conductivity
  • Resists chemical attack
  • Unaffected by oil or water
  • Completely inorganic
  • Excellent acoustical properties
  • Applications:

  • Fill, void, or cavity material in through-penetration seals (firestops)
  • Seal duct, cable bundle, conduit, tubing, and cable tray penetrations
  • Information provided by Thermal Ceramics

    Available Properties
    • Melting Point
    • Maximum Service Temperature, Air
    • Flammability Test
    • Water Leachable Elements on Surface of Fiber, PPM
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
    请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

    本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。